Acetal: Acetal (POM) Copolymer
Product | Availability | Product Description |
---|---|---|
TES AC-80/GB/20/M BK | Africa & Middle East | |
TES J-80/10 BK223 | Africa & Middle East | |
TES J-80/10 NAT | Africa & Middle East | |
TES J-80/10 | Africa & Middle East |
Molding Parameters:
For 2-zone machines, the rear temperature is 360-410°F, and the front temperature is 350-380°F.
|
TES J-80/20 | Africa & Middle East |
Molding Parameters:
For 2-zone machines, the rear temperature is 360-410°F, and the front temperature is 350-380°F.
|
TexRes ACETAL COPO BLACK | North America |
Acetal Copolymer, General Purpose Injection Grade
Colors Available
Add "U" for UV Stabilized
|
Titacon® CF910 | Asia Pacific |
10%CARBON FIBER REINFORCED, WEAR RESISTANCE, HIGH STIFFNESS/STRENGTH.
|
Titacon® CF920 | Asia Pacific |
20%CARBON FIBER REINFORCED, WEAR RESISTANCE, HIGH STIFFNESS/STRENGTH
|
Titacon® CW901 | Asia Pacific |
CHEMICAL LUBRICATION, WEAR RESISTANCE, LOW SPEED/HIGH LOAD APPLICATION.
|
Titacon® EW901 | Asia Pacific |
CHEMICAL LUBRICATION, HIGH SPEED/LOW LOAD APPLICATION, LOW NOISE.
|
Titacon® EX210 | Asia Pacific |
EXTRUSION GRADE, PERMANENT ANTI-STATIC, CARBON BLACK.
|
Titacon® EX910 | Asia Pacific |
INJECTION MOLDING GRADE, PERMANENT ANTI-STATIC, CARBON BLACK.
|
Titacon® GB910L | Asia Pacific |
10% GLASS BEADS FILLED, LOW WARPAGE, SURFACE LUBRICATED.
|
Titacon® GB915 | Asia Pacific |
15% GLASS BEADS FILLED DIMENSIONAL ACCURACY LOWER WARPAGE
|
Titacon® GB920 | Asia Pacific |
20% GLASS BEADS FILLED LOWER WARPAGE
|
Titacon® GB925 | Asia Pacific |
25% GLASS BEADS FILLED, DIMENSIONAL ACCURACY, LOWER WARPAGE.
|
Titacon® GF910 | Asia Pacific |
10%GLASS FIBER REINFORCED, HIGH STRENGTH/STIFFNESS, DIMENSIONAL ACCURACY.
|
Titacon® GF915 | Asia Pacific |
15%GLASS FIBER FILLED, HIGH STRENGTH/STIFFNESS.
|
Titacon® GF920 | Asia Pacific |
20% GLASS FIBER REINFORCED HIGH STRENGTH STIFFNESS
|
Titacon® GF920TF10 | Asia Pacific |
20%GLASS FIBER REINFORCED, 10%PTFE FILLED, HIGH STRENGTH/STIFFNESS, DIMENSIONAL ACCURACY, WEAR RESISTANCE.
|
Titacon® GF925 | Asia Pacific |
25% GLASS FIBER REINFORCED, HIGH STRENGTH/STIFFNESS, DIMENSIONAL ACCURACY.
|
Titacon® GF925TF10 | Asia Pacific |
25%GLASS FIBER REINFORCED, 10%PTFE FILLED, HIGH STRENGTH/STIFFNESS, DIMENSIONAL ACCURACY, WEAR RESISTANCE.
|
Titacon® GF925UV | Asia Pacific |
25%GLASS FIBER REINFORCED, HIGH STRENGTH/STIFFNESS, WEATHER RESISTANCE.
|
Titacon® GF930 | Asia Pacific |
30% GLASS FIBER REINFORCED, HIGH STRENGTH/STIFFNESS, DIMENSIONAL ACCURACY.
|
Titacon® KG920 | Asia Pacific |
20%WHISKER FILLED, WEAR RESISTANCE, HIGH STIFFNESS.
|
Titacon® MS902 | Asia Pacific |
2.5%MOLYBDENUM DISULFIDE FILLED, WEAR RESISTANCE, MEDIUM FLOW.
|
Titacon® MS904 | Asia Pacific |
4%MOLYBDENUM DISULFIDE FILLED, WEAR RESISTANCE, MEDIUM FLOW.
|
Titacon® NC940 | Asia Pacific |
PERMANENT ANTI-STATIC, CARBON NANOTUBE FILLED.
|
Titacon® NW901 | Asia Pacific |
CHEMICAL LUBRICATION, LOW WEAR/FRICTION, LOW NOISE.
|
Titacon® SI902 | Asia Pacific |
2%SILICONE FILLED, LOW FRICTION, MEDIUM FLOW.
|
Titacon® ST220 | Asia Pacific |
EXTRUSION GRADE, PERMANENT ANTI-STATIC, NON-SLOUGHING, WEAR RESISTANCE, COLORABLE.
|
Titacon® ST915 | Asia Pacific |
INJECTION MOLDING GRADE, PERMANENT ANTI-STATIC, NON-SLOUGHING, WEAR RESISTANCE, IMPACT MODIFIED, COLORABLE.
|
Titacon® TF905 | Asia Pacific |
5%PTFE POWDER FILLED, WEAR RESISTANCE, MEDIUM FLOW.
|
Titacon® TF905S2 | Asia Pacific |
5%PTFE /2%SILICONE FILLED, WEAR RESISTANCE, MEDIUM FLOW.
|
Titacon® TF910 | Asia Pacific |
10%PTFE POWDER FILLED, WEAR RESISTANCE, MEDIUM FLOW.
|
Titacon® TF918K7 | Asia Pacific |
PTFE / ARAMID FIBER FILLED, WEAR RESISTANCE, LOW FRICTION, NON-ABRASIVE TO METAL.
|
Titacon® TF920 | Asia Pacific |
20%PTFE POWDER FILLED, WEAR RESISTANCE.
|
Titacon® TR720 | Asia Pacific |
15% TALC FILLED HIGH STIFFNESS LOW WARPAGE DIMENSIONAL ACCURACY MEDIUM FLOW
|
Titacon® TR905 | Asia Pacific |
5%TALC FILLED, LOW WARPAGE, DIMENSIONAL ACCURACY, MEDIUM FLOW.
|
Titacon® TX910 | Asia Pacific |
IMPACT MODIFIED, TOUGHNESS, MEDIUM FLOW.
|