Policarbonato (PC): HiFill FR®
Producto | Disponibilidad | Descripción del producto |
---|---|---|
HiFill FR® J-50/20/FR | África y Oriente Medio |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 550-590°F, and the front temperature is 540-560°F.
|
HiFill FR® J-50/30/FR | África y Oriente Medio |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 550-590°F, and the front temperature is 540-560°F.
|
HiFill FR® PC 1001 FR-NR | Norteamérica | |
HiFill FR® PC 1003 FR-NR UV | Norteamérica | |
HiFill FR® PC 1003 UV | Norteamérica | |
HiFill FR® PC FR 06 NAT | Norteamérica | |
HiFill FR® PC FR IM | Norteamérica | |
HiFill FR® PC GF10 FR BK | Norteamérica | |
HiFill FR® PC IM FR | Norteamérica | |
HiFill FR® PC MCF/GB 1525 BK001 | Norteamérica | |
HiFill FR® PC/ABS FR NH | Norteamérica |