RTV-2 P-FDA
P-FDA is mixed 100 parts of Base to 10 parts of Activator by weight. Deviations from this ratio will cause changes in the physical properties. Choose a container with a volume that is four times greater than that of the rubber. Weigh the components accurately and mix thoroughly. Since there is no color, mix very carefully, scraping the sides and bottom of the container to insure that there is no unmixed portion. Place the container in a vacuum chamber and deaerate at 28 inches of mercury vacuum until the mass of rubber rises and then collapses.
一般属性
使用 Prospector 建立免費帳戶時,可造訪 RTV-2 P-FDA 的完整資料表詳細資訊。您將找到有關物理、機械和硬度規格的完整資訊
Technical Datasheet (English)
下载文档加工
Find specific processing information for RTV-2 as well as general information for the Silicone Rubber, RTV-2 generic family. 注册 或 登录 了解更多信息。