乙缩醛 (Acetal): Kepital®
产品 | 可用性 | 产品说明 |
---|---|---|
Kepital® AF-11 | 北美洲 |
POM, aramid powder-filled wear-resistance
- Aaramid powder-filled wear-resistance grade for general injection molding - Suitable for parts requiring strong friction and wear resistance, particularly in contact with other plastics
|
Kepital® ED-10 | 北美洲 |
- An anti-static high-viscosity grade for general extrusion molding (rods, plates, sheets, etc.)
- Suitable for applications requiring surface resistivity 10E9 ohm
- Cautions
-- Surface resistivity will change with extrusion conditions: die design, pressure, speed, etc.
-- In addition, color shade will change with product thickness, retention time, and annealing conditions.
|
Kepital® ET-20A BK | 北美洲 |
- A conductive grade for general injection molding
- Features superior toughness and fuel-contact resistance
- Suitable for automotive fuel module parts
|
Kepital® ET-20A | 北美洲 |
A carbon black filled, conductive grade
Carbon black filled conductive grade and surface resistivity is less than 104 Ohm. It has good fuel and chemical resistance and it’s suitable for fuel module parts.
|
Kepital® ET-20R3 BK | 北美洲 |
POM, CNT filled, high viscosity, conductive and anti-static, for extrusion molding
- A CNT filled high-viscosity grade for general extrusion molding (rods, plates, sheets, etc.) - Suitable for applications requiring surface resistivity 103 Ohm - Cautions: Surface resistivity will change with extrusion conditions: die design, pressure, seeed, etc.
|
Kepital® ET-20R7 BK | 北美洲 |
POM, CNT filled, conductive and anti-static, for extrusion molding
- A CNT (Carbon Nano Tube) filled anti-static grade for general extrusion molding (rods, plates, sheets, etc.) - Suitable for electric and automotive parts requiring anti-static property - Cautions: Surface resistivity will change with extrusion conditions: die design, pressure, seeed, etc.
|
Kepital® ET-20R7G BK | 北美洲 |
POM, CNT filled, conductive and anti-static, for extrusion molding
- A CNT (Carbon Nano Tube) filled anti-static grade for general extrusion molding (rods, plates, sheets, etc.) - Suitable for electric and automotive parts requiring anti-static property - Cautions: Surface resistivity will change with extrusion conditions: die design, pressure, seeed, etc.
|
Kepital® ET-20S | 北美洲 |
- A conductive grade for general injection molding
- Suitable for applications requiring electrical conductivity
|
Kepital® F10-01 T2 BBK | 北美洲 |
a high-viscosity grade for extrusion of round bars, sheets and tubes; a blended material with black master batch.
KEPITAL® F10-01 T2 BBK is a high-viscosity grade for extrusion of round bars, sheets and tubes Suitable for uses requiring high productivity without micro porosity for large diameter rods and plates. A blended material with black master batch.
|
Kepital® F10-01 T2 | 北美洲 |
a high-viscosity grade for extrusion of round bars, sheets and tubes
KEPITAL® F10-01 T2 is a high-viscosity grade for extrusion of round bars, sheets and tubes Suitable for uses requiring high productivity without micro porosity for large diameter rods and plates.
|
Kepital® F10-01 | 北美洲 |
- A high-viscosity grade for extrusion of round bars, sheets and tubes
- Suitable for extrusion molding of thick-walled, void-free, and sink mark-reduced parts
|
Kepital® F10-02 | 北美洲 |
- A high-viscosity grade for extrusion of round bars, sheets, and tubes
- Suitable for extrusion molding of thick-walled, void-free, and sink mark-reduced parts
|
Kepital® F10-03H LOF | 北美洲 |
- A stiffness-improved(high-viscosity) grade for general injection molding.
- A low-emission grade featuring thermal stability.
- Features greater stiffness compared to general POM copolymer.
|
Kepital® F10-03H | 北美洲 |
- A high-viscosity grade for general injection molding
- It has a high stiffness compared to general POM copolymer.
|
Kepital® F10-03HM | 北美洲 |
POM, copolymer, unfilled, stiffness-improved, high-viscosity
- A stiffness-improved (high-viscosity) grade for general injection molding. - Features greater stiffness compared to general POM copolymer. - Improved resistance to heat, high humidity, hot water
|
Kepital® F10-52D | 北美洲 |
A UV-stabilized high-viscosity grade for general injection molding
-Â A UV-stabilized high-viscosity grade for general injection molding.
|
Kepital® F10-52H LOF | 北美洲 |
POM, UV-stabilized, high-viscosity, low emission
-Â A UV-stabilized high-viscosity grade for general injection molding. - Developed for applications in automotive interiors and exposed part - A low-emission grade featuring improved heat stability
|
Kepital® F10-52H | 北美洲 |
POM, UV-stabilized, high-viscosity
-Â A UV-stabilized high-viscosity grade for general injection molding. - Developed for applications in automotive interiors and exposed part
|
Kepital® F15-33 | 北美洲 |
- A toughness-improved(medium-high viscosity)grade for general injection molding.
- Features improved toughness and molding cycle time
|
Kepital® F20-02 | 北美洲 |
POM, medium-viscosity
- A medium-viscosity grade for general injection molding
|
Kepital® F20-03 BLW | 北美洲 |
a medium-viscosity grade for general injection molding. Suitable for applications requiring laser welding
KEPITAL® F20-03 BLW is a medium-viscosity grade for general injection molding. Suitable for applications requiring laser welding.
|
Kepital® F20-03 Colored | 北美洲 |
a medium-viscosity grade for general injection molding (colored)
Kepital® F20-03 Colored is a medium-viscosity grade for general injection molding (colored). A general grade for injection molding applications.
|
Kepital® F20-03 LOF | 北美洲 |
- A low-emission (medium-viscosity) grade for general injection molding.
- Features improved heat stability.
|
Kepital® F20-03 LOF2 | 北美洲 |
POM, unfilled, low emission, low-to-medium viscosity, improved heat stability
A low-emission (low-to-medium viscosity) grade for general injection molding. Features improved heat stability.
|
Kepital® F20-03 | 北美洲 |
- A medium-viscosity grade for general injection molding
|
Kepital® F20-03M | 北美洲 |
a medium-viscosity grade for general injection molding. Features improved resistance in hot water and high temperature/humidity.
KEPITAL® F20-03M is a medium-viscosity grade for general injection molding. Features improved resistance in hot water and high temperature/humidity.
|
Kepital® F20-33 | 北美洲 |
POM, unfilled, medium viscosity, improved toughness
A toughness-improved (medium viscosity) grade for general injection molding. Features: improved molding cycle, toughness and wear resistance
|
Kepital® F20-51 | 北美洲 |
- A UV-stabilized medium-viscosity grade for general injection molding (black-colored)
- Suitable for uses requiring strong weather resistance
- Developed for applications in automotive exteriors and exposed parts
|
Kepital® F20-51U | 北美洲 |
- A UV-stabilized and impact-improved medium-viscosity grade for general injection molding (black-colored)
- Suitable for uses requiring strong weather resistance
- Developed for applications in automotive exteriors and exposed parts
|
Kepital® F20-52 LOF | 北美洲 |
- A UV-stabilized (medium-viscosity) grade for general injection molding
- A low-emission grade featuring improved heat stability
- Developed for applications in automotive interiors
|
Kepital® F20-52 LOF2 | 北美洲 |
POM, unfilled, medium viscosity, UV stabilized, low emission, improved heat stability
A UV-stabilized (medium-viscosity) grade for general injection molding. A low-emission grade featuring improved heat stability Developed for application in automotive interiors or exteriors
|
Kepital® F20-52 | 北美洲 |
- A UV-stabilized medium-viscosity grade for general injection molding
- Developed for applications in automotive interiors and exposed parts
|
Kepital® F20-52G | 北美洲 |
- A UV-stabilized and gloss-reduced, medium-viscosity grade for general injection molding
- Modified with a weather-resistant and gloss-reducing substance
- Suitable for applications requiring strong weather resistance and low gloss characteristics
|
Kepital® F25-03 LOF | 北美洲 |
- A medium-low viscosity grade for general injection molding
- A low-emission grade featuring improved thermal stability
|
Kepital® F25-03 | 北美洲 |
- A medium-low viscosity grade for general injection molding
|
Kepital® F25-03H | 北美洲 |
- A stiffness-improved(medium-viscosity) grade for general injection molding.
- It has a high stiffness compared to general POM copolymer.
|
Kepital® F25-03HT LOF | 北美洲 |
POM, low emission, a friction & wear-resistance (medium-viscosity) grade for general injection molding
- Kepital® F25-03HT LOF is a friction & wear-resistance (medium-viscosity) grade for general injection molding. -Â Suitable for applications requiring reduced impact noise and good friction and wear resistance. - A low-emission grade featured improved heat stability.
|
Kepital® F25-03HT | 北美洲 |
A friction & wear-resistance (medium-viscosity) grade for general injection molding
Kepital® F25-03HT is a friction & wear-resistance (medium-viscosity) grade for general injection molding. Suitable for applications requiring reduced impact noise and good friction and wear resistance.
|
Kepital® F25-63 | 北美洲 |
An anti-static, medium-low viscosity grade for general injection molding
Anti-static, medium-low viscosity grade in general injection molding purpose.
|
Kepital® F30-03 LOF | 北美洲 |
- A low-viscosity grade for general injection molding
- A low-emission grade featuring thermal stability
- Suitable for multi-cavity molds and thin-walled parts
|