聚碳酸酯(PC): PC+ABS

产品 可用性 产品说明
TAIRILOY® AC2300 北美洲
General Purpose Grade CHARACTERISTICS: Metal plating
TAIRILOY® AC2500 北美洲
General Purpose Grade CHARACTERISTICS: Heat resistant
TAIRILOY® AC25BM 北美洲
Extrusion & Blow Molding CHARACTERISTICS: Extrusion & Blow Molding
TAIRILOY® AC3100 北美洲
Self Extinguishing Grade CHARACTERISTICS: Flame retardant Cl, Br, Sb free.
TAIRILOY® AC3250 北美洲
Self Extinguishing Grade CHARACTERISTICS: Flame retardant, Halogen free
TAIRILOY® AC3300 北美洲
Self Extinguishing Grade CHARACTERISTICS: Flame retardant, Halogen free
TARFLON™ SC-170 北美洲
For plating
TARFLON™ SC-253 北美洲
For plating
TARFLON™ SK2706 北美洲
High flow, Standard
TARFLON™ SK2708 北美洲
High flow, High impact
TAROBLEND 30 欧洲
PC/ABS alloy medium low thermal resistance, good flow.
TAROBLEND 45 X0 欧洲  
TAROBLEND 45 欧洲
PC/ABS alloy medium thermal resistance, good flow and mechanical properties. FORD TL 522 31 (Type A) Available: all colors, UV-stablized (L), antistatic (AS).
TAROBLEND 46 欧洲  
TAROBLEND 50 X0 欧洲  
TAROBLEND 60 X0 欧洲
PC/ABS alloy self extinguishing UL94 V0, medium thermal resistance, improved thermal stability, low halogen content, without antimony trioxide. UL94 approved V0 all colors at 1,7 mm. UL746B approved. Available: different colours.
TAROBLEND 65 X0 欧洲  
TAROBLEND 65 欧洲
PC/ABS alloy medium-high thermal resistance, good flow and mechanical properties, low moisture absorption and good dimensional stability. FIAT CR 110.500 - FORD TL 522 31 (Type B) Available: all colors, UV stabilized (L).
TAROBLEND 66 X0 欧洲
PC/ABS alloy good thermal resistance, flame retardant UL94 V0, improved thermal stability and UV light resistance, Bromine, Chlorine and Antimony compounds free.
TAROBLEND 66 欧洲
PC/ABS alloy medium-high thermal resistance, very good flow and mechanical properties, low moisture absorption and good dimensional stability.
TAROBLEND 85 X0 欧洲
PC/ABS alloy self extinguishing UL94 V0, high thermal resistance, good mechanical properties and dimensional stability. UL94 approved V0 all colors at 1,7 mm. UL746B approved. Available: all colors.
TAROBLEND 85 欧洲
PC/ABS alloy high thermal resistance, good flow and very high mechanical properties, low moisture absorption and good dimensional stability. Available: all colors, UV stabilized (L).
TAROBLEND 86 欧洲  
TAROBLEND 88 G2 欧洲
PC/ABS alloy glass fiber reinforced 10%. Available: all colors, UV stabilized (L).
TAROBLEND 88 G4 欧洲
PC/ABS alloy 20% glass fibres reinforced, high stiffness and thermal resistance.
TECHNIACE® F-101 北美洲  
TECHNIACE® H-261 北美洲  
TECHNIACE® H-270 北美洲  
TECHNIACE® PAX-1427 北美洲  
TECHNIACE® PAX-1439 北美洲  
TECHNO ALPHALOY MPC2501LG 北美洲  
TECHNO ALPHALOY MPC6801 北美洲  
TECHNOGRAN® ABSPCI 欧洲  
Tecotek® BC40 UF45 NL CE 非洲和中东
PC/ABS, unfilled, heat & UV stabilized, natural, easy flow grade
Tecotek® BC40 UF65 NL CE 非洲和中东
PC/ABS, unfilled, heat & UV stabilized, natural, standard grade
Tecotek® BC40 UF85 NL CE 非洲和中东
PC/ABS, unfilled, heat & UV stabilized, natural, high heat grade
Tecotek® BC43 UF65 NL CE 非洲和中东
PC/ABS, unfilled, heat & UV stabilized, natural, standard grade
TEKALOY™ G70A2 亚太地区
Features - G70A2 is a PC/ABS alloy unreinforced product. Application - E/E parts. Drying - Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
TEKALOY™ G70A3 亚太地区
Features - G70A3 is a PC/ABS alloy unreinforced with heat resistance. Application - E/E parts. Drying - Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.
TEKALOY™ G70A4 亚太地区
Features - TEKALOY G70A4 is unreinforced PC/ABS alloy. Application - Miscellaneous Goods Drying - Product is dried and packed with a moisture content of <0.16%. Should the Packaging become damaged or be left open too long, then the material must be Dried. A too high moisture content can lead to a reduction of optical and Mechanical properties.