Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 550-590°F, and the front temperature is 540-560°F.
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 550-590°F, and the front temperature is 540-560°F.